Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.37 g/cm³ Show Supplier Material materials with Dichte of 1.37 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.83 % Show Supplier Material materials with Moisture absorption of 0.83 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.35 [-] Show Supplier Material materials with Relative Dichte of 1.35 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 157 MPa Show Supplier Material materials with Biegefestigkeit of 157 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 6.8 GPa Show Supplier Material materials with Biegemodul of 6.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 8.1 % Show Supplier Material materials with Dehnung of 8.1 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 9.7 GPa Show Supplier Material materials with Elastizitätsmodul of 9.7 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 106 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 727 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 727 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 16 J Show Supplier Material materials with Instrumented Impact, at Peak of 16 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 10 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 53 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 53 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 35 MPa Show Supplier Material materials with Zugfestigkeit of 35 MPa | ISO 527 | yield, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 141 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 141 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 135 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 70 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 70 °C | UL 746B | |
Relative temperature index, mechanical strength | 85 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 85 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 135 - 141 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 135 - 141 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093413- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 1 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 1 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 0 V Show Supplier Material materials with Kriechstromfestigkeit of 0 V | UL 746A | (UL) {PLC} |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |