Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.51 - 0.52 [-] Show Supplier Material materials with Coefficient of friction of 0.51 - 0.52 [-] | ||
Coefficient of friction, kinetic | 0.51 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.51 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.52 [-] Show Supplier Material materials with Coefficient of friction, static of 0.52 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 2.2 g/cm³ Show Supplier Material materials with Dichte of 2.2 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 137 MPa Show Supplier Material materials with Biegefestigkeit of 137 MPa | ISO 178 |
Biegemodul | 23.0 °C | 14.9 GPa Show Supplier Material materials with Biegemodul of 14.9 GPa | ISO 178 |
Dehnung | 23.0 °C | 0.8 % Show Supplier Material materials with Dehnung of 0.8 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 16.3 GPa Show Supplier Material materials with Elastizitätsmodul of 16.3 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 16 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 16 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 170 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 170 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 4 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 14 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Zugfestigkeit | 23.0 °C | 84 MPa Show Supplier Material materials with Zugfestigkeit of 84 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 264 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 264 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 202 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 202 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 202 - 264 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 202 - 264 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 1.05 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1.05 W/(m·K) | ASTM E 1530 | | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101343423- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 0 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 0 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Supplier Material materials with Kriechstromfestigkeit of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, Data Transfer, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |