Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.34 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.97 % Show Supplier Material materials with Moisture absorption of 0.97 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.34 [-] Show Supplier Material materials with Relative Dichte of 1.34 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 159 MPa Show Supplier Material materials with Biegefestigkeit of 159 MPa | ISO 178 |
Biegemodul | 23.0 °C | 5 GPa Show Supplier Material materials with Biegemodul of 5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2.7 % Show Supplier Material materials with Dehnung of 2.7 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 5.5 GPa Show Supplier Material materials with Elastizitätsmodul of 5.5 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 46 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 46 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 393 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 393 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 6 J Show Supplier Material materials with Instrumented Impact, Total Energy of 6 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 4 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 25 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 103 MPa Show Supplier Material materials with Zugfestigkeit of 103 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 257 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 257 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 240 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 240 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.7E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 240 - 257 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 240 - 257 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.6E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344610- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Modular Panel, Medical Device | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |