Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.41 - 0.57 [-] Show Supplier Material materials with Coefficient of friction of 0.41 - 0.57 [-] | ||
Coefficient of friction, kinetic | 0.57 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.57 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.41 [-] Show Supplier Material materials with Coefficient of friction, static of 0.41 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.68 g/cm³ Show Supplier Material materials with Dichte of 1.68 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | ISO 62 | (23°C / 50% RH) |
Wasserabsorption | 23.0 °C | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | ISO 62-1 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 183 MPa Show Supplier Material materials with Biegefestigkeit of 183 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 8.9 GPa Show Supplier Material materials with Biegemodul of 8.9 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2.8 % Show Supplier Material materials with Dehnung of 2.8 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 10.1 GPa Show Supplier Material materials with Elastizitätsmodul of 10.1 GPa | ISO 527 | 1 mm/min |
Flexural strain | 23.0 °C | 3.1 % Show Supplier Material materials with Flexural strain of 3.1 % | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 750 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 750 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 13 J Show Supplier Material materials with Instrumented Impact, at Peak of 13 J | ASTM D 3763 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 9 kJ/m² | ISO 180/1A | notched 80*10*3, -40°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 60 kJ/m² | ISO 180/1U | unnotched 80*10*4, -40°C |
Zugfestigkeit | 23.0 °C | 114 MPa Show Supplier Material materials with Zugfestigkeit of 114 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 222 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 222 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 208 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 208 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 75 °C Show Supplier Material materials with Relative temperature index, electrical of 75 °C | UL 746B | |||
Relative temperature index, mechanical impact | 75 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 75 °C | UL 746B | |||
Relative temperature index, mechanical strength | 75 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 75 °C | UL 746B | |||
Spezifische Wärmekapazität | 23.0 °C | 1751 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 1751 J/(kg·K) | ASTM E 1269 | ||
Vicat-Erweichungstemperatur | 212 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 212 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 208 - 222 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 208 - 222 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.26 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.26 W/(m·K) | ASTM D 5930 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.7E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282605- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103093711- - <br> UL Yellow Card Link 3: https://iq.ul.com/ul/cert.aspx?ULID=101282616- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 22 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 22 g/10min | ASTM D 1238 | 250°C/5.0 kgf | |
Schmelzvolumenflussrate | 17 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 17 cm³/10min | ISO 1133 | MVR at 250°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | SABIC method |
Schrumpfung, diagonal | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung, diagonal of 0.5 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Commercial Appliance, Data Management, Data Transfer, Displays, Electronic Components, Electronics, Heavy Vehicles, Gear/Bearing/Slider, Engine Component, Medical Device, Oil/Gas, Personal Computing, Security/Detection, Pharmaceutical Packaging & Drug Delivery, Pallet | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |