Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.18 - 0.23 [-] Show Supplier Material materials with Coefficient of friction of 0.18 - 0.23 [-] | ||
Coefficient of friction, kinetic | 0.23 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.23 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.18 [-] Show Supplier Material materials with Coefficient of friction, static of 0.18 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Relative Dichte | 23.0 °C | 1.14 [-] Show Supplier Material materials with Relative Dichte of 1.14 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 77 MPa Show Supplier Material materials with Biegefestigkeit of 77 MPa | ISO 178 | ||
Biegemodul | 23.0 °C | 2.1 GPa Show Supplier Material materials with Biegemodul of 2.1 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 4.9 % Show Supplier Material materials with Dehnung of 4.9 % | ISO 527 | yield, 50 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.1 GPa Show Supplier Material materials with Elastizitätsmodul of 2.1 GPa | ISO 527 | 1 mm/min | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 654 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 654 J/m | ASTM D 256 | notched, 23°C | ||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 39 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 39 kJ/m² | ISO 179/2C | -30°C | ||
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 48 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 48 kJ/m² | ISO 180/1A | 80*10*4, 23°C | ||
Zugfestigkeit | 23.0 °C | 49 MPa Show Supplier Material materials with Zugfestigkeit of 49 MPa | ISO 527 | yield, 5 mm/min | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C | ||||
Schlagzähigkeit, Izod ungekerbt | ISO 180/1U | unnotched 80*10*4 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 125 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 110 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 110 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.3E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.3E-5 1/K | ASTM D 696 | -30°C to 30°C |
Wärmeformbeständigkeitstemperatur | 110 - 125 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 110 - 125 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.8E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.8E-5 1/K | ASTM D 696 | -30°C to 30°C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 30 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 30 g/10min | ASTM D 1238 | 260°C/5.0 kgf | |
Schrumpfung | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | ASTM D 955 | 24 hrs |
Schrumpfung, diagonal | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung, diagonal of 0.6 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Infotainment/Telematic, Panels | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 95 to 105.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |