Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.162 g/cm³ Show Supplier Material materials with Dichte of 1.162 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 155 MPa Show Supplier Material materials with Biegefestigkeit of 155 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 4 GPa Show Supplier Material materials with Biegemodul of 4 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % | ASTM D 638 | brk, Type I, 5 mm/min |
Zugfestigkeit | 23.0 °C | 89 MPa Show Supplier Material materials with Zugfestigkeit of 89 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.9E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.9E-5 1/K | ASTM E 831 | -20°C to 150°C |
Vicat-Erweichungstemperatur | 240 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 240 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Auto Electrical, Electronic Components, Enclosures, Enclosure/Housing/Cover, Exterior Trim, Forward Lighting, Fixture Bath/Shower, Fog Lamp, Lab Ware and Clinical Diagnostics, Lawn/Garden, Individual Equiptment, Recreational Vehicle, Power Boat, Pipe/Fitting, Rear/Signal Lighting, Photo/Video Camera, Plumbing, Wireless Communications | |
Availability | Europe,Asia,MEA,Americas | |
Processing methods | Rear - Zone 1 Temperature: 265 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |