Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.162 g/cm³ Show Supplier Material materials with Dichte of 1.162 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 1.18 % Show Supplier Material materials with Moisture absorption of 1.18 % | ISO 62 | (23°C / 50% RH) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 165 MPa Show Supplier Material materials with Biegefestigkeit of 165 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 3.9 GPa Show Supplier Material materials with Biegemodul of 3.9 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | ISO 527 | break, 5 mm/min |
Zugfestigkeit | 23.0 °C | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | ISO 527 | yield, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.4E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Vicat-Erweichungstemperatur | 221 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 221 °C | ISO 306 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Auto Electrical, Electronic Components, Enclosures, Enclosure/Housing/Cover, Exterior Trim, Forward Lighting, Fixture Bath/Shower, Fog Lamp, Lab Ware and Clinical Diagnostics, Lawn/Garden, Individual Equiptment, Recreational Vehicle, Power Boat, Pipe/Fitting, Rear/Signal Lighting, Photo/Video Camera, Plumbing, Wireless Communications | |
Availability | Europe,Asia,MEA,Americas | |
Processing methods | Back Pressure: 0.3 to 1.4MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |