Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Dichte of 1.45 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.03 % Show Supplier Material materials with Moisture absorption of 0.03 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 366 MPa Show Supplier Material materials with Biegefestigkeit of 366 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 25 GPa Show Supplier Material materials with Biegemodul of 25 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 1.8 % Show Supplier Material materials with Dehnung of 1.8 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 23.5 GPa Show Supplier Material materials with Elastizitätsmodul of 23.5 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 70 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 70 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 775 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 775 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 70 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 70 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 270 MPa Show Supplier Material materials with Zugfestigkeit of 270 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 341 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 341 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 327 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 327 °C | ASTM D 648 | 3.2mm, unannealed |
Wärmeformbeständigkeitstemperatur | 327 - 341 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 327 - 341 °C |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |