Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.52 g/cm³ Show Supplier Material materials with Dichte of 1.52 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 186 MPa Show Supplier Material materials with Biegefestigkeit of 186 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 9.8 GPa Show Supplier Material materials with Biegemodul of 9.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 11.7 GPa Show Supplier Material materials with Elastizitätsmodul of 11.7 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 140 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 140 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 521 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 521 J/m | ASTM D 4812 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 140 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 140 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 143 MPa Show Supplier Material materials with Zugfestigkeit of 143 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 114 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 114 °C | ASTM D 648 | 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.54E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.54E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 114 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 114 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5.63E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5.63E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101265025- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.8mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥0.6mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 57 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 57 g/10min | ASTM D 1238 | 300°C/5.0 kgf | |
Schmelzvolumenflussrate | 14 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 14 cm³/10min | ISO 1133 | MVR at 300°C/2.16 kg | |
Schrumpfung | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | ASTM D 955 | 24 hrs |
Schrumpfung, diagonal | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung, diagonal of 0.1 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Wireless Communications, Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |