Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.22 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Wasserabsorption | 23.0 °C | 0.01 % Show Supplier Material materials with Wasserabsorption of 0.01 % | ASTM D 570 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 79 MPa Show Supplier Material materials with Biegefestigkeit of 79 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 75 % Show Supplier Material materials with Dehnung of 75 % | ASTM D 638 | brk, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Elastizitätsmodul of 2.4 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 550 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 550 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 550 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 46 MPa Show Supplier Material materials with Zugfestigkeit of 46 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 106 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 106 °C | ASTM D 648 | 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.1E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 106 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 106 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100974177- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.6mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.94 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.94 [-] | IEC 60250 |
Dissipation factor, 1GHz | 23.0 °C | 5.7E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 5.7E-3 [-] | IEC 60250 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 14 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 14 cm³/10min | ISO 1133 | MVR at 260°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | ASTM D 955 | 24 hrs |
Schrumpfung, diagonal | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung, diagonal of 0.6 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Data Transfer, Enclosures, Electronic Components, Wireless Communications, Vacuum Cleaner | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 85 to 95.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |