Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.32 g/cm³ Show Supplier Material materials with Dichte of 1.32 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 130 MPa Show Supplier Material materials with Biegefestigkeit of 130 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 5.8 GPa Show Supplier Material materials with Biegemodul of 5.8 GPa | ISO 178 | 2 mm/min |
Elastizitätsmodul | 23.0 °C | 6.2 GPa Show Supplier Material materials with Elastizitätsmodul of 6.2 GPa | ISO 527 | 1 mm/min |
Flexural strain | 23.0 °C | 2.5 % Show Supplier Material materials with Flexural strain of 2.5 % | ISO 178 | break, 2 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 23 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 23 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | IEC 60695-2-13 | 2.0 mm | |
Heat deflection temperature, 1.80 MPa | 118 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 118 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Vicat-Erweichungstemperatur | 130 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 130 °C | ISO 306 | Rate B/120 | |
Wärmeformbeständigkeitstemperatur | 118 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 118 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284052- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 825°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 8 cm³/10min | ISO 1133 | MVR at 260°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | SABIC method |
Schrumpfung, diagonal | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung, diagonal of 0.3 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80 to 90.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |