Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.21 [-] Show Supplier Material materials with Relative Dichte of 1.21 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Biegefestigkeit of 80 MPa | ASTM D 790 | yield, 6.4 mm |
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 200 % Show Supplier Material materials with Dehnung of 200 % | ISO 527 | break, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 700 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 700 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 700 kJ/m² | ASTM D 256 | notched, 23°C |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 100 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 100 °C | ASTM D 648 | 6.4 mm, unannealed | |
Wärmeformbeständigkeitstemperatur | 100 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 100 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228454- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥0.5mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.20E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.20E+12 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 19 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 19 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 1.5-3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung, diagonal of 0.5 % | SABIC method | 1.5-3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Pallet, Photo/Video Camera, Data Management, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 100.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |