Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 206 MPa Show Supplier Material materials with Biegefestigkeit of 206 MPa | ASTM D 790 | yield, 6.4 mm |
Biegemodul | 23.0 °C | 11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | ASTM D 790 | 6.4 mm |
Dehnung | 23.0 °C | 9.7 % Show Supplier Material materials with Dehnung of 9.7 % | SABIC - Japan Method | brk, Type I, 10 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 93 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 93 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 93 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 93 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 141 MPa Show Supplier Material materials with Zugfestigkeit of 141 MPa | SABIC - Japan Method | yld, Type I, 10 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 199 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 199 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 199 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 199 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236836- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥0.5mm UL 94 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 36.4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 36.4 g/10min | ASTM D 1238 | 250°C/5.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |