Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.49 - 0.73 [-] Show Supplier Material materials with Coefficient of friction of 0.49 - 0.73 [-] | ||
Coefficient of friction, kinetic | 0.49 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.49 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.73 [-] Show Supplier Material materials with Coefficient of friction, static of 0.73 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.64 g/cm³ Show Supplier Material materials with Dichte of 1.64 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 263 MPa Show Supplier Material materials with Biegefestigkeit of 263 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 11.4 GPa Show Supplier Material materials with Biegemodul of 11.4 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 12.2 GPa Show Supplier Material materials with Elastizitätsmodul of 12.2 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 103 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 103 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 861 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 861 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 13 J Show Supplier Material materials with Instrumented Impact, Total Energy of 13 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 103 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 103 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 177 MPa Show Supplier Material materials with Zugfestigkeit of 177 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 337 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 337 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 322 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 322 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Wärmeformbeständigkeitstemperatur | 322 - 337 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 322 - 337 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 3.6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 3.6E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283797- - <br> UL Recognized, 94V-0 Flame Class Rating: 0.8mm UL 94 |
Technological properties
Property | ||
---|---|---|
Application areas | Oil/Gas, Medical Device | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |