Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Dichte of 1.19 g/cm³ | ASTM D 792 |
Relative Dichte | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative Dichte of 1.2 [-] | ASTM D 792 | |
Specific volume | 23.0 °C | 0.83 cm³/g Show Supplier Material materials with Specific volume of 0.83 cm³/g | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.35 % Show Supplier Material materials with Wasserabsorption of 0.35 % | ASTM D 570 | (23°C/Saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 93 MPa Show Supplier Material materials with Biegefestigkeit of 93 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 110 % Show Supplier Material materials with Dehnung of 110 % | ASTM D 638 | brk, Type I, 50 mm/min |
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Supplier Material materials with Hardness, Rockwell R of 118 [-] | ASTM D 785 |
Härte, Rockwell M | 23.0 °C | 70 [-] Show Supplier Material materials with Härte, Rockwell M of 70 [-] | ASTM D 785 | |
Impact strength, Izod notched, ASTM | 23.0 °C | 907 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 907 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 3204 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 907 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 907 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Zugfestigkeit | 23.0 °C | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 137 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 132 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 132 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.84E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.84E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Spezifische Wärmekapazität | 23.0 °C | 1.26E-3 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 1.26E-3 J/(kg·K) | ASTM C 351 | ||
Vicat-Erweichungstemperatur | 154 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 154 °C | ASTM D 1525 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 132 - 137 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 132 - 137 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.29 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.29 W/(m·K) | ASTM C177 | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103952989- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 3.17 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.17 [-] | ASTM D 150 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.96 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.96 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 9E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 9E-4 [-] | ASTM D 150 | 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 15 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 15 kV/mm | ASTM D 149 | in air, 3.2 mm |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | ASTM D 257 |
Optisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |