Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 457 MPa Show Supplier Material materials with Biegefestigkeit of 457 MPa | ISO 178 |
Biegemodul | 23.0 °C | 27.2 GPa Show Supplier Material materials with Biegemodul of 27.2 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.5 % Show Supplier Material materials with Dehnung of 1.5 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 35.3 GPa Show Supplier Material materials with Elastizitätsmodul of 35.3 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 75 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 75 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 936 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 936 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 6 J Show Supplier Material materials with Instrumented Impact, Total Energy of 6 J | ASTM D 3763 | 23°C |
Poissonzahl | 23.0 °C | 0.4 [-] Show Supplier Material materials with Poissonzahl of 0.4 [-] | ASTM E 132 |
Scherfestigkeit | 23.0 °C | 119 MPa Show Supplier Material materials with Scherfestigkeit of 119 MPa | ASTM D732 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 75 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 75 kJ/m² | ASTM D 256 | notched, 23°C |
Schubmodule | 23.0 °C | 4.8 GPa Show Supplier Material materials with Schubmodule of 4.8 GPa | ASTM D732 |
Zugfestigkeit | 23.0 °C | 319 MPa Show Supplier Material materials with Zugfestigkeit of 319 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 332 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 332 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5E-6 1/K | ASTM E 831 | -40°C to 150°C |
Wärmeformbeständigkeitstemperatur | 332 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 332 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 3E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 3E-5 1/K | ASTM E 831 | -40°C to 150°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1000 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1000 - 10000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |