Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 460 MPa Show Supplier Material materials with Biegefestigkeit of 460 MPa | ISO 178 |
Biegemodul | 23.0 °C | 33.8 GPa Show Supplier Material materials with Biegemodul of 33.8 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.4 % Show Supplier Material materials with Dehnung of 1.4 % | ISO 527 | break, 5 mm/min |
Druckfestigkeit | 23.0 °C | 215 MPa Show Supplier Material materials with Druckfestigkeit of 215 MPa | SABIC method |
Elastizitätsmodul | 23.0 °C | 40.4 GPa Show Supplier Material materials with Elastizitätsmodul of 40.4 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 82 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 82 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 863 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 863 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 7 J Show Supplier Material materials with Instrumented Impact, Total Energy of 7 J | ASTM D 3763 | 23°C |
Poissonzahl | 23.0 °C | 0.5 [-] Show Supplier Material materials with Poissonzahl of 0.5 [-] | ASTM E 132 |
Scherfestigkeit | 23.0 °C | 126 MPa Show Supplier Material materials with Scherfestigkeit of 126 MPa | ASTM D732 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 82 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 82 kJ/m² | ASTM D 256 | notched, 23°C |
Schubmodule | 23.0 °C | 5 GPa Show Supplier Material materials with Schubmodule of 5 GPa | ASTM D732 |
Zugfestigkeit | 23.0 °C | 321 MPa Show Supplier Material materials with Zugfestigkeit of 321 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Aerospace | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |