Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.66 g/cm³ Show Supplier Material materials with Dichte of 1.66 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 60 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 60 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 60 kJ/m² | ASTM D 256 | notched, 23°C |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 134 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 134 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 122 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C | ASTM D 648 | 3.2mm, unannealed |
Wärmeformbeständigkeitstemperatur | 122 - 134 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 122 - 134 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 4.4 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 4.4 [-] | ASTM ES 7-83 | 1.1 GHz |
Dissipation factor, 1GHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 2E-3 [-] | ASTM ES 7-83 | 1.1 GHz |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 11 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 11 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | ASTM D 955 | 24 hrs |
Schrumpfung, diagonal | 23.0 °C | 0.65 % Show Supplier Material materials with Schrumpfung, diagonal of 0.65 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Wiring Devices, Cooking Range | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 105°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |