Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.236 g/cm³ Show Supplier Material materials with Dichte of 1.236 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 92 MPa Show Supplier Material materials with Biegefestigkeit of 92 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 16.5 % Show Supplier Material materials with Dehnung of 16.5 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastizitätsmodul of 2.6 GPa | ISO 527 | 1 mm/min |
Flexural strain | 23.0 °C | 7.8 % Show Supplier Material materials with Flexural strain of 7.8 % | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 359 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 359 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2140 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 2140 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 39 J Show Supplier Material materials with Instrumented Impact, Total Energy of 39 J | ASTM D 3763 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 27 J Show Supplier Material materials with Instrumented Impact, at Peak of 27 J | ASTM D 3763 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 26 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 26 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 24 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 24 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 130 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 130 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 58 MPa Show Supplier Material materials with Zugfestigkeit of 58 MPa | ISO 527 | yield, 5 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Vicat-Erweichungstemperatur | 144 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 144 °C | ISO 306 | Rate A/50 |
Wärmeformbeständigkeitstemperatur | 126 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 126 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 4.80E+7 Ω Show Supplier Material materials with Sheet resistivity, ROA of 4.80E+7 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.41E+7 Ω·cm Show Supplier Material materials with Volume resistivity of 1.41E+7 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 16 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 16 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.64 % Show Supplier Material materials with Schrumpfung of 0.64 % | SABIC method | 1.5-3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.68 % Show Supplier Material materials with Schrumpfung, diagonal of 0.68 % | SABIC method | 1.5-3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Semiconductor, LED Lighting, Enclosures, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |