Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.32 g/cm³ Show Supplier Material materials with Dichte of 1.32 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 90 kJ/m² | ASTM D 256 | notched, 23°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 19 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 19 cm³/10min | ISO 1133 | MVR at 300°C/3.8 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |