Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Moisture absorption | 23.0 °C | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Relative Dichte | 23.0 °C | 1.24 [-] Show Supplier Material materials with Relative Dichte of 1.24 [-] | ASTM D 792 | |
Sauerstoffindex | 23.0 °C | 26 % Show Supplier Material materials with Sauerstoffindex of 26 % |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 174 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 174 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.6E-5 1/K | ASTM D 696 | -30°C to 30°C |
Wärmeformbeständigkeitstemperatur | 174 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 174 °C |
Elektrisch
Technological properties
Property | ||
---|---|---|
Application areas | Monitoring and Imaging, Medical Device | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |