Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.28 g/cm³ Show Supplier Material materials with Dichte of 1.28 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.89 % Show Supplier Material materials with Moisture absorption of 0.89 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.28 [-] Show Supplier Material materials with Relative Dichte of 1.28 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.1 GPa Show Supplier Material materials with Biegemodul of 0.1 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 388 % Show Supplier Material materials with Dehnung of 388 % | ASTM D 638 | yld, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 0.1 GPa Show Supplier Material materials with Elastizitätsmodul of 0.1 GPa | ASTM D 638 | 5 mm/min |
Instrumented Impact, Total Energy | 23.0 °C | 39 J Show Supplier Material materials with Instrumented Impact, Total Energy of 39 J | ASTM D 3763 | 23°C |
Zugfestigkeit | 23.0 °C | 19 MPa Show Supplier Material materials with Zugfestigkeit of 19 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 23 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 23 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm |
Heat deflection temperature, 1.80 MPa | 23 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 23 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Wärmeformbeständigkeitstemperatur | 23 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 23 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 100000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 100000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |