Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 106 MPa Show Supplier Material materials with Biegefestigkeit of 106 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.7 GPa Show Supplier Material materials with Biegemodul of 2.7 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 50 - 100 % Show Supplier Material materials with Dehnung of 50 - 100 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 70.3 MPa Show Supplier Material materials with Zugfestigkeit of 70.3 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 174 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 174 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.6E-5 1/K | ASTM D 696 | -30°C to 30°C |
Wärmeformbeständigkeitstemperatur | 174 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 174 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1MHz | 23.0 °C | 3.02 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3.02 [-] | ASTM D 150 | |
Dissipation factor, 1kHz | 23.0 °C | 3.04 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 3.04 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 3.03 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 3.03 [-] | ASTM D 150 | 50/60 Hz |
Volume resistivity | 23.0 °C | 5.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 5.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 17 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 17 g/10min | ASTM D 1238 | 330°C/2.16 kgf | |
Schrumpfung | 23.0 °C | 0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Others, Surgical Tray, Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 135 to 163.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |