Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.27 [-] Show Supplier Material materials with Relative Dichte of 1.27 [-] | ASTM D 792 | |
Sauerstoffindex | 23.0 °C | 47 % Show Supplier Material materials with Sauerstoffindex of 47 % | |
Wasserabsorption | 23.0 °C | 1.25 % Show Supplier Material materials with Wasserabsorption of 1.25 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 160 MPa Show Supplier Material materials with Biegefestigkeit of 160 MPa | ISO 178 | yield, 2 mm/min | ||
Biegemodul | 23.0 °C | 3.3 GPa Show Supplier Material materials with Biegemodul of 3.3 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 60 % Show Supplier Material materials with Dehnung of 60 % | ISO 527 | break, 50 mm/min | ||
Elastizitätsmodul | 23.0 °C | 3.2 GPa Show Supplier Material materials with Elastizitätsmodul of 3.2 GPa | ISO 527 | 1 mm/min | ||
Gardner Impact | 23.0 °C | 33 J Show Supplier Material materials with Gardner Impact of 33 J | SABIC method | ||
Hardness, Ball Indentation | 23.0 °C | 140 MPa Show Supplier Material materials with Hardness, Ball Indentation of 140 MPa | ISO 2039-1 | H358/30 | ||
Härte, Rockwell M | 23.0 °C | 109 [-] Show Supplier Material materials with Härte, Rockwell M of 109 [-] | ASTM D 785 | | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 32 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 32 J/m | ASTM D 256 | ||
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1335 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1335 J/m | ASTM D 4812 | 23°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 33 J Show Supplier Material materials with Instrumented Impact, Total Energy of 33 J | ASTM D 3763 | 23°C | ||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C | ||
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C | ||
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg | ||
Zugfestigkeit | 23.0 °C | 105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | ISO 527 | yield, 50 mm/min | ||
Schlagzähigkeit, Izod ungekerbt | ISO 180/1U | 80*10*4, 23°C |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Passes | IEC 60695-10-2 | 125°C +/- 2°C | |||
Heat deflection temperature, 0.45 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 200 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 190 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Vicat-Erweichungstemperatur | 212 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 212 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 190 - 200 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 - 200 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.21 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.21 W/(m·K) | ISO 8302 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Entflammbarkeit | Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.9 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.9 [-] | IEC 60250 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.9 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.9 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 6E-3 [-] | IEC 60250 |
Dissipation factor, 1kHz | 23.0 °C | 1.3E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 1.3E-3 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 5E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 5E-4 [-] | IEC 60250 | 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 33 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 33 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
Kriechstromfestigkeit | 23.0 °C | 100 V Show Supplier Material materials with Kriechstromfestigkeit of 100 V | IEC 60112 | M |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Verlustfaktor | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Verlustfaktor of 2.5E-3 [-] | IEC 60250 | 2450 MHz |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 17.8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 17.8 g/10min | ASTM D 1238 | 337°C/6.6 kgf | |
Schmelzvolumenflussrate | 25 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 25 cm³/10min | ISO 1133 | MVR at 360°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | on tensile bar |
Schrumpfung, diagonal | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung, diagonal of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Food Processor, Food Transportation, Gas/Electric Oven, Head Protection, Electronic Components, Airline Service, Animal Testing, Commercial Storage/Cookware, Coffee Maker/Espresso Machine, Small Appliance, Servingware, LED Lighting, Medical Device, Surgical Tray | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 345 to 400.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |