Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.28 - 0.35 [-] Show Supplier Material materials with Coefficient of friction of 0.28 - 0.35 [-] | ||
Coefficient of friction, kinetic | 0.35 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.35 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.28 [-] Show Supplier Material materials with Coefficient of friction, static of 0.28 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.43 g/cm³ Show Supplier Material materials with Dichte of 1.43 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 276 MPa Show Supplier Material materials with Biegefestigkeit of 276 MPa | ISO 178 |
Biegemodul | 23.0 °C | 14.7 GPa Show Supplier Material materials with Biegemodul of 14.7 GPa | ISO 178 |
Dehnung | 23.0 °C | 2.9 % Show Supplier Material materials with Dehnung of 2.9 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 14.5 GPa Show Supplier Material materials with Elastizitätsmodul of 14.5 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 7 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 34 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 34 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 162 MPa Show Supplier Material materials with Zugfestigkeit of 162 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.36E-5 1/K | ISO 11359-2 | -40°C to 40°C |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5.3E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5.3E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Technological properties
Property | ||
---|---|---|
Application areas | Surgical Devices | |
Availability | Europe,Americas | |
Processing methods | Back Pressure: 0.3 to 0.7MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |