Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0 GPa Show Supplier Material materials with Biegemodul of 0 GPa | ISO 178 | 12.5 mm/min |
Dehnung | 23.0 °C | 260 % Show Supplier Material materials with Dehnung of 260 % | ISO 527 | break, 50 mm/min |
Härte, Shore A | 23.0 °C | 81 [-] Show Supplier Material materials with Härte, Shore A of 81 [-] | ASTM D 2240 | 30S reading |
Zugfestigkeit | 23.0 °C | 17 MPa Show Supplier Material materials with Zugfestigkeit of 17 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 3.0 mm | |
Entflammbarkeit | Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 166- ASTM E 662 <br> Smoke Density on 0.5mm plaque, Flame, Ds, max: 117- ASTM E 662 <br> Glow Wire Flammability Index 850°C, passes at: 3mm IEC 60695-2-12 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 5GHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 5GHz of 2.6 [-] | SABIC method |
Dissipation factor, 5GHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 5GHz of 2E-3 [-] | SABIC method |
Durchschlagfestigkeit | 23.0 °C | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | ASTM D 149 | in oil |
Kriechstromfestigkeit | 23.0 °C | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 | |
Sheet resistivity, ROA | 23.0 °C | 1.60E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.60E+16 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 5.10E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 5.10E+15 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 10 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 10 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Drying Temperature: 75 to 85.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |