Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | ISO 1183 |
Relative Dichte | 23.0 °C | 1.13 [-] Show Supplier Material materials with Relative Dichte of 1.13 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 105 MPa Show Supplier Material materials with Biegefestigkeit of 105 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ISO 527 | yield, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.7 GPa Show Supplier Material materials with Elastizitätsmodul of 2.7 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 220 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 220 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 18 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 18 kJ/m² | ISO 179/2C | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 10 kJ/m² | ISO 180/1A | notched 80*10*4 |
Zugfestigkeit | 23.0 °C | 57 MPa Show Supplier Material materials with Zugfestigkeit of 57 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 0.45 MPa | 136 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 136 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 123 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 123 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL 746B | |||
Relative temperature index, mechanical impact | 125 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 125 °C | UL 746B | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 155 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 155 °C | ISO 306 | Rate A/120 | |||
Wärmeformbeständigkeitstemperatur | 123 - 136 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 123 - 136 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100960629- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1mm UL 94 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 825°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F1- UL 746C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1 mm Show Supplier Material materials with High Amp Arc Ignition of 1 mm | ≥, UL 746A | PLC 1 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1 mm Show Supplier Material materials with Hot-Wire Ignition of 1 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 4 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Schmelzvolumenflussrate | 8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 8 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management, Electronic Components, Photovoltaic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 105°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |