Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Dichte of 1.19 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ISO 178 | 1.3 mm/min |
Dehnung | 23.0 °C | 7 % Show Supplier Material materials with Dehnung of 7 % | ISO 527 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 1.8 GPa Show Supplier Material materials with Elastizitätsmodul of 1.8 GPa | ISO 527 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 170 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 | notched, -30°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1000 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1000 J/m | ASTM D 256 | un-notched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 10 J Show Supplier Material materials with Instrumented Impact, Total Energy of 10 J | ASTM D 3763 | -30 °C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | ISO 179 | notched, 23°C |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 88 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 88 kJ/m² | ISO 179 | un-notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 18 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 18 kJ/m² | ISO 180 | notched, 23°C, |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 22 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 22 kJ/m² | ISO 180 | un-notched, -30°C |
Zugfestigkeit | 23.0 °C | 49 MPa Show Supplier Material materials with Zugfestigkeit of 49 MPa | ISO 527 | brk, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 137 °C | ISO 75 | 3.2 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.7E-5 1/K | ASTM E 831 | ||
Vicat-Erweichungstemperatur | 149 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 149 °C | ISO 306 | Rate A/50 | |||
Wärmeformbeständigkeitstemperatur | 137 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 137 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 77 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 77 1/K | ASTM E 831 | ||
Entflammbarkeit | UL94 Flame Class Rating: V-0- UL 94 <br> UL94 Flame Class Rating: V-0- UL 94 <br> UL94 Flame Class Rating: V-2- UL 94 <br> UL94 Flame Class Rating: V-2- UL 94 <br> UL94 Flame Class Rating: V-2- UL 94 <br> UL94 Flame Class Rating: V-2- UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.6 [-] | ASTM D150 |
Verlustfaktor | 23.0 °C | 5E-3 [-] Show Supplier Material materials with Verlustfaktor of 5E-3 [-] | ASTM D 150 | |
Volume resistivity | 23.0 °C | 1.50E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.50E+15 Ω·cm | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Plastic | |
Availability | Europe,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |