Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 129 MPa Show Supplier Material materials with Biegefestigkeit of 129 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 5.6 GPa Show Supplier Material materials with Biegemodul of 5.6 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 7.7 % Show Supplier Material materials with Dehnung of 7.7 % | ASTM D 638 | brk, Type I, 5 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 165 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 165 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 79 MPa Show Supplier Material materials with Zugfestigkeit of 79 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 155 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 155 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 133 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.44E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.44E-5 1/K | ASTM E 831 | -40°C to 40°C |
Vicat-Erweichungstemperatur | 162 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 162 °C | ASTM D 1525 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 133 - 155 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 133 - 155 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.74E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.74E-5 1/K | ASTM E 831 | -40°C to 40°C |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Power Boat, Weapon, Water Treatment/Filtration, Vacuum Cleaner, Furnace/Heater, Hot Water System, Enclosures, Electronic Components, Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 250 to 290.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |