Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Dichte of 1.4 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.4 [-] Show Supplier Material materials with Relative Dichte of 1.4 [-] | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 195 MPa Show Supplier Material materials with Biegefestigkeit of 195 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 9.5 GPa Show Supplier Material materials with Biegemodul of 9.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.8 % Show Supplier Material materials with Dehnung of 1.8 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 11.3 GPa Show Supplier Material materials with Elastizitätsmodul of 11.3 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 | notched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 18 J Show Supplier Material materials with Instrumented Impact, Total Energy of 18 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 108 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 108 kJ/m² | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 30 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 155 MPa Show Supplier Material materials with Zugfestigkeit of 155 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 147 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 147 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Vicat-Erweichungstemperatur | 161 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 161 °C | ISO 306 | Rate B/120 | |
Wärmeformbeständigkeitstemperatur | 147 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 147 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 10 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 10 g/10min | ASTM D 1238 | 300°C/5.0 kgf | |
Schmelzvolumenflussrate | 20 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 20 cm³/10min | ISO 1133 | MVR at 300°C/10.0 kg | |
Schrumpfung | 23.0 °C | 0.09 % Show Supplier Material materials with Schrumpfung of 0.09 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Pump, Pipe/Fitting | |
Availability | Europe,Asia,Americas | |
Processing methods | Mold Temperature: 80 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |