Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.19 [-] Show Supplier Material materials with Relative Dichte of 1.19 [-] | ASTM D 792 | |
Wasserabsorption | 23.0 °C | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 96 MPa Show Supplier Material materials with Biegefestigkeit of 96 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 90 % Show Supplier Material materials with Dehnung of 90 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastizitätsmodul of 2.6 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 175 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 175 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 65 J Show Supplier Material materials with Instrumented Impact, Total Energy of 65 J | ASTM D 3763 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 40 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 40 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 10 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C |
Zugfestigkeit | 23.0 °C | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Pass | IEC 60695-10-2 | 75°C +/- 2°C | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 1.80 MPa | 93 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 93 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 90 °C Show Supplier Material materials with Relative temperature index, electrical of 90 °C | UL 746B | |||
Relative temperature index, mechanical impact | 90 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |||
Relative temperature index, mechanical strength | 90 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 90 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 113 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 113 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 93 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 93 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=564206- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 35 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 35 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | UL 746A | PLC 3 |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Supplier Material materials with Kriechstromfestigkeit of 3 V | UL 746A | (UL) {PLC} |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 18 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 18 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Schmelzvolumenflussrate | 15 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 15 cm³/10min | ISO 1133 | MVR at 260°C/2.16 kg | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, Monitoring and Imaging, Meter Gas, Medical Facility Infrastructure, Personal Computing, Respiratory, Surgical Devices, Pharmaceutical Packaging & Drug Delivery, Photo/Video Camera, Power Manangement, Wireless Communications, Enclosures, Energy Management, Electronic Components, Lab Ware and Clinical Diagnostics, Fluid Delivery, Displays, Data Management, Cooking Range, Animal Testing, Building Accessory | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80 to 90.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |