Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.22 [-] Show Supplier Material materials with Relative Dichte of 1.22 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 102 MPa Show Supplier Material materials with Biegefestigkeit of 102 MPa | ASTM D 790 | yield, 6.4 mm |
Biegemodul | 23.0 °C | 4.6 GPa Show Supplier Material materials with Biegemodul of 4.6 GPa | ASTM D 790 | 6.4 mm |
Dehnung | 23.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 35 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 35 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 35 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 103 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 103 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.2E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 103 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 103 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4.8E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 4.8E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100140832- - |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 24 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 24 g/10min | ASTM D 1238 | 300°C/2.16 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Asia | |
Processing methods | Rear - Zone 1 Temperature: 220 to 270.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |