Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative Dichte of 1.2 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 89 MPa Show Supplier Material materials with Biegefestigkeit of 89 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 65 % Show Supplier Material materials with Dehnung of 65 % | ASTM D 638 | brk, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 550 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 65 J Show Supplier Material materials with Instrumented Impact, Total Energy of 65 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 550 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 550 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 63 MPa Show Supplier Material materials with Zugfestigkeit of 63 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 78 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 78 °C | ASTM D 648 | 3.2mm, unannealed |
Vicat-Erweichungstemperatur | 102 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 102 °C | ASTM D 1525 | Rate B/50 |
Wärmeformbeständigkeitstemperatur | 78 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 78 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 26 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 26 g/10min | ASTM D 1238 | 266°C/5.0 kgf | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Power Manangement, Safety Glasses, Renal and Blood Handling, Medical Facility Infrastructure, Monitoring and Imaging, Medical Device, Navigation Unit, Personal Computing, Watch/Jewelry, Wearables, Wireless Communications, Vending Machine, Displays, Audio, Enclosure/Housing/Cover, Enclosures, Electronic Components, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Shot to Cylinder Size: 30 to 80.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |