Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.11 g/cm³ Show Supplier Material materials with Dichte of 1.11 g/cm³ | ISO 1183 |
Relative Dichte | 23.0 °C | 1.11 [-] Show Supplier Material materials with Relative Dichte of 1.11 [-] | ASTM D 792 | |
Sauerstoffindex | 23.0 °C | 30 % Show Supplier Material materials with Sauerstoffindex of 30 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 71 MPa Show Supplier Material materials with Biegefestigkeit of 71 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ISO 527 | yield, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 38 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 38 J/m | ASTM D 256 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 3 kJ/m² | ISO 180/1A | 80*10*4, -30°C |
Zugfestigkeit | 23.0 °C | 46 MPa Show Supplier Material materials with Zugfestigkeit of 46 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 93 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 93 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 77 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 77 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 101 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 101 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 77 - 93 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 77 - 93 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.9E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.9E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94V-1 Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101313034- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.7 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 2.9E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2.9E-3 [-] | IEC 60250 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 17 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 17 cm³/10min | ISO 1133 | MVR at 280°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Availability | Europe | |
Processing methods | Nozzle Temperature: 250 to 280.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |