Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 104 MPa Show Supplier Material materials with Biegefestigkeit of 104 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | ISO 527 | yield, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastizitätsmodul of 2.6 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 170 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 55 J Show Supplier Material materials with Instrumented Impact, Total Energy of 55 J | ASTM D 3763 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, -30°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Zugfestigkeit | 23.0 °C | 67 MPa Show Supplier Material materials with Zugfestigkeit of 67 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 2.0 mm | |
Heat deflection temperature, 0.45 MPa | 128 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 128 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 111 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 111 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |
Vicat-Erweichungstemperatur | 144 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 144 °C | ISO 306 | Rate A/120 | |
Wärmeformbeständigkeitstemperatur | 111 - 128 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 111 - 128 °C | ||
Entflammbarkeit | Glow Wire Ignitability Temperature, 1.5 mm: 800°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101401128- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥2mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 49 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 49 kV/mm | ASTM D 149 | in air, 3.2 mm |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Volume resistivity | 23.0 °C | 1.40E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.40E+17 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt viscosity | 23.0 °C | 250 Pa·s Show Supplier Material materials with Melt viscosity of 250 Pa·s | ISO 11443 | 280°C, 1500 sec-1 |
Schmelzvolumenflussrate | 7 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 7 cm³/10min | ISO 1133 | MVR at 250°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Refrigerator, Washing Machine, Air Conditioning, Gas/Electric Oven, Enclosure/Housing/Cover | |
Availability | Asia | |
Processing methods | Middle - Zone 2 Temperature: 255 to 300.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |