Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.6 g/cm³ Show Supplier Material materials with Dichte of 1.6 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 285 MPa Show Supplier Material materials with Biegefestigkeit of 285 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 10.6 GPa Show Supplier Material materials with Biegemodul of 10.6 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 3.7 % Show Supplier Material materials with Dehnung of 3.7 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 15.5 GPa Show Supplier Material materials with Elastizitätsmodul of 15.5 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 19 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 19 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 95 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 95 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 181 MPa Show Supplier Material materials with Zugfestigkeit of 181 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 203 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 203 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | ASTM E 831 | -40°C to 40°C |
Wärmeformbeständigkeitstemperatur | 203 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 203 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.8E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.8E-5 1/K | ASTM E 831 | -40°C to 40°C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.18 % Show Supplier Material materials with Schrumpfung of 0.18 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors, Electronic Components, Heavy Vehicles | |
Availability | Europe,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |