Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.34 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.11 % Show Supplier Material materials with Moisture absorption of 0.11 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.34 [-] Show Supplier Material materials with Relative Dichte of 1.34 [-] | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.28 % Show Supplier Material materials with Wasserabsorption of 0.28 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 107 MPa Show Supplier Material materials with Biegefestigkeit of 107 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 109 % Show Supplier Material materials with Dehnung of 109 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 194 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 194 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 80 J Show Supplier Material materials with Instrumented Impact, Total Energy of 80 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 194 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 194 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 74 MPa Show Supplier Material materials with Zugfestigkeit of 74 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball pressure temperature | 125 °C Show Supplier Material materials with Ball pressure temperature of 125 °C | IEC 60695-10-2 | approximate maximum | |||
Heat deflection temperature, 1.80 MPa | 117 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 117 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Vicat-Erweichungstemperatur | 139 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 139 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 117 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 117 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | Vertical Burn b (12s) passes at: 0.5sec FAR 25.853 <br> Vertical Burn a (60s) passes at: 2.4sec FAR 25.853 <br> OSU peak heat release rate (5 minute test): <55kW/m² FAR 25.853 <br> NBS Smoke Density, Flaming, Dmax: <25- ASTM E 662 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 5 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Schmelzvolumenflussrate | 16 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 16 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Aircraft Seating, Aerospace, Air Cabin Interiors, Rail Window Glazing, Sensor, Rail Seating, Personal Computing | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 280 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |