Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Dichte of 1.19 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.18 [-] Show Supplier Material materials with Relative Dichte of 1.18 [-] | ASTM D 792 |
Sauerstoffindex | 23.0 °C | 35 % Show Supplier Material materials with Sauerstoffindex of 35 % | |
Wasserabsorption | 23.0 °C | 0.35 % Show Supplier Material materials with Wasserabsorption of 0.35 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 85 MPa Show Supplier Material materials with Biegefestigkeit of 85 MPa | ISO 178 | yield, 2 mm/min | ||
Biegemodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | ISO 527 | yield, 50 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | ISO 527 | 1 mm/min | ||
Hardness, Rockwell L | 23.0 °C | 89 [-] Show Supplier Material materials with Hardness, Rockwell L of 89 [-] | ASTM D 785 | ||
Hardness, Rockwell R | 23.0 °C | 121 [-] Show Supplier Material materials with Hardness, Rockwell R of 121 [-] | ASTM D 785 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 774 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 774 J/m | ASTM D 256 | ||
Instrumented Impact, Total Energy | 23.0 °C | 70 J Show Supplier Material materials with Instrumented Impact, Total Energy of 70 J | ASTM D 3763 | 23°C | ||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 65 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 65 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 60 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Zugfestigkeit | 23.0 °C | 57 MPa Show Supplier Material materials with Zugfestigkeit of 57 MPa | ISO 527 | yield, 50 mm/min | ||
Schlagzähigkeit, Charpy ungekerbt | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C | ||||
Schlagzähigkeit, Izod ungekerbt | ISO 180/1U | 80*10*3, -30°C |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Passes | IEC 60695-10-2 | 125°C +/- 2°C | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 875 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 875 °C | IEC 60695-2-13 | 0.8 mm | |||
Heat deflection temperature, 0.45 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 140 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 128 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 128 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.2E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 145 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 145 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 128 - 140 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 128 - 140 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.2E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100079875- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=228376- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.0 mm: 875°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 0.8 mm: 850°C IEC 60695-2-12 <br> UV-light, water exposure/immersion: F1- UL 746C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.64 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.64 [-] | ASTM D 150 |
Dielektrizitätskonstante, 100 Hz | 23.0 °C | 2.68 [-] Show Supplier Material materials with Dielektrizitätskonstante, 100 Hz of 2.68 [-] | ASTM D 150 |
Dissipation factor, 100Hz | 23.0 °C | 1.2E-3 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 1.2E-3 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 9.3E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 9.3E-3 [-] | ASTM D 150 |
Durchschlagfestigkeit | 23.0 °C | 16.2 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 16.2 kV/mm | ASTM D 149 | in oil, 0.8 mm |
High Amp Arc Ignition | 23.0 °C | 0.7 mm Show Supplier Material materials with High Amp Arc Ignition of 0.7 mm | ≥, UL 746A | PLC 1 |
Hot-Wire Ignition | 23.0 °C | 0.7 mm Show Supplier Material materials with Hot-Wire Ignition of 0.7 mm | ≥, UL 746A | PLC 0 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 10 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 10 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Schmelzvolumenflussrate | 9 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 9 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung, diagonal of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wearables, Watch/Jewelry, Water Treatment/Filtration, Wiring Devices, Wireless Communications, Surgical Tray, Travel Suitcase, Vending Machine, Vacuum Cleaner, LED Lighting, Medical Device, Monitoring and Imaging, Medical Facility Infrastructure, Personal Care, Motorcycle, Non-LED Lighting, Personal Computing, Smart/ID Card, Small Appliance, Power Manangement, Photovoltaic Components, Photo/Video Camera, Refrigerator, Circuit Protection, Audio, Auto Aftermarket, Air Conditioning, Data Transfer, Data Management, Body Protection, Cooking Range, Displays, Document Handling, Electronic Components, Enclosures, Enclosure/Housing/Cover, Electronics, Head Protection, Fuel Handling, Heavy Vehicles, Lab Ware and Clinical Diagnostics, Lawn/Garden, Infotainment/Telematic, Furnace/Heater, Eyeglasses, EV Infrastructure, Irrigation | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |