Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.06 g/cm³ Show Supplier Material materials with Dichte of 1.06 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Wasserabsorption | 23.0 °C | 0.19 % Show Supplier Material materials with Wasserabsorption of 0.19 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 45 MPa Show Supplier Material materials with Biegefestigkeit of 45 MPa | ISO 178 | yield, 2 mm/min |
Dehnung | 23.0 °C | 55 % Show Supplier Material materials with Dehnung of 55 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 1.5 GPa Show Supplier Material materials with Elastizitätsmodul of 1.5 GPa | ISO 527 | 1 mm/min |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, -30°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 25 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 30 MPa Show Supplier Material materials with Zugfestigkeit of 30 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 75°C +/- 2°C | |||
Heat deflection temperature, 0.45 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 115 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 105 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 105 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Vicat-Erweichungstemperatur | 120 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 120 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 105 - 115 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 105 - 115 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.22 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.22 W/(m·K) | ISO 8302 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 9E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 9E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Entflammbarkeit | UL Compliant, 94HB Flame Class Rating: 1.6mm UL 94 by SABIC-IP |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.7 [-] | IEC 60250 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.6 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 9E-4 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 9E-4 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 4E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 4E-4 [-] | IEC 60250 | 50/60 Hz |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 12 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 12 cm³/10min | ISO 1133 | MVR at 280°C/10.0 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Data Transfer, Wire & cable | |
Availability | Europe | |
Processing methods | Hopper Temperature: 60 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |