Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 93 MPa Show Supplier Material materials with Biegefestigkeit of 93 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 6.2 % Show Supplier Material materials with Dehnung of 6.2 % | ASTM D 638 | yld, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Elastizitätsmodul of 2.4 GPa | ASTM D 638 | 50 mm/min |
Zugfestigkeit | 23.0 °C | 48 MPa Show Supplier Material materials with Zugfestigkeit of 48 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 132 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 132 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 121 °C | ASTM D 648 | 3.2mm, unannealed |
Wärmeformbeständigkeitstemperatur | 121 - 132 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 121 - 132 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Personal Computing, Medical Device, Respiratory, Enclosures, Forward Lighting, Document Handling | |
Availability | Europe,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |