Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 152 MPa Show Supplier Material materials with Biegefestigkeit of 152 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 8.2 GPa Show Supplier Material materials with Biegemodul of 8.2 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 7 % Show Supplier Material materials with Dehnung of 7 % | SABIC - Japan Method | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 68 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 68 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 68 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 68 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 108 MPa Show Supplier Material materials with Zugfestigkeit of 108 MPa | SABIC - Japan Method | yield |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.4E-5 - 3.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 - 3.4E-5 1/K | TMA | -30°C to 30°C | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 125 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 125 °C | ||||
Entflammbarkeit | UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥2mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228542- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.25 % Show Supplier Material materials with Schrumpfung of 0.25 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures, Document Handling, Displays, Personal Computing | |
Availability | Asia | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |