Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.275 g/cm³ Show Supplier Material materials with Dichte of 1.275 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | ASTM D 790 | 1.3 mm/min |
Dehnung | 23.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ASTM D638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 2.8 GPa Show Supplier Material materials with Elastizitätsmodul of 2.8 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 31 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 31 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 273 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 273 J/m | ASTM D 256 | un-notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 31 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 31 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | ASTM D638 | brk, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 211 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 211 °C | ASTM D648 | 3.2 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.3E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.3E-5 1/K | ASTM E 831 | ||
Vicat-Erweichungstemperatur | 220 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 220 °C | ASTM D 1525 | |||
Wärmeformbeständigkeitstemperatur | 211 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 211 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 52 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 52 1/K | ASTM E 831 | ||
Entflammbarkeit | UL94 Flame Class Rating: 5VA- UL 94 <br> UL94 Flame Class Rating: V0- UL 94 <br> UL94 Flame Class Rating: V0- UL 94 <br> UL94 Flame Class Rating: V0- UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.94 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.94 [-] | ASTM D150 |
Verlustfaktor | 23.0 °C | 3E-3 [-] Show Supplier Material materials with Verlustfaktor of 3E-3 [-] | ASTM D150 |
Volume resistivity | 23.0 °C | 1.26E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.26E+15 Ω·cm | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Plastic, Fused Deposition Modeling (FDM), Healthcare | |
Availability | Europe,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |