Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Moisture absorption | 23.0 °C | 0.02 % Show Supplier Material materials with Moisture absorption of 0.02 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.1 [-] Show Supplier Material materials with Relative Dichte of 1.1 [-] | ASTM D 792 | |
Wasserabsorption | 23.0 °C | 0.13 % Show Supplier Material materials with Wasserabsorption of 0.13 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 98 MPa Show Supplier Material materials with Biegefestigkeit of 98 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.8 GPa Show Supplier Material materials with Biegemodul of 2.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 7.3 % Show Supplier Material materials with Dehnung of 7.3 % | ASTM D 638 | brk, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 3.1 GPa Show Supplier Material materials with Elastizitätsmodul of 3.1 GPa | ASTM D 638 | 50 mm/min |
Zugfestigkeit | 23.0 °C | 52 MPa Show Supplier Material materials with Zugfestigkeit of 52 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.4E-5 1/K | ISO 11359-2 | -40°C to 40°C |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.4E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.4E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+14 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+14 Ω | IEC 60093 |
Volume resistivity | 23.0 °C | 4.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 4.00E+16 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 34 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 34 cm³/10min | ISO 1133 | MVR at 280°C/2.16 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Displays, Washing Machine | |
Availability | Europe | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |