Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 89 MPa Show Supplier Material materials with Biegefestigkeit of 89 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 52 % Show Supplier Material materials with Dehnung of 52 % | ASTM D 638 | brk, Type I, 50 mm/min |
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Supplier Material materials with Hardness, Rockwell R of 118 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 272 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 272 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 3204 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 36 J Show Supplier Material materials with Instrumented Impact, at Peak of 36 J | ASTM D 3763 | -30 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 272 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 272 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 19 mg/1000cy Show Supplier Material materials with Taber Abrasion of 19 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Zugfestigkeit | 23.0 °C | 56 MPa Show Supplier Material materials with Zugfestigkeit of 56 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 155 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 155 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 127 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 127 °C | ASTM D 648 | 6.4 mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9E-5 1/K | ASTM E 831 | -20°C to 150°C |
Vicat-Erweichungstemperatur | 232 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 232 °C | ASTM D 1525 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 127 - 155 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 127 - 155 °C |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Applique, Power Boat, Recreational Vehicle, Motorcycle, Laundry Dryer, Weapon, Vertical Body Panel, Wheel Cover, Washing Machine, Exterior Rail Components, Engine Component, Exterior Mirror, Exterior Trim, Heavy Vehicles, Lawn/Garden, Enclosures, Cowl Vent Grille, Door Handle, Building Accessory, Auto Electrical, Auto Aftermarket | |
Availability | Asia,Americas | |
Processing methods | Melt Temperature: 275 to 300.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |