Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 49 MPa Show Supplier Material materials with Biegefestigkeit of 49 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 1.3 GPa Show Supplier Material materials with Biegemodul of 1.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 120 % Show Supplier Material materials with Dehnung of 120 % | ASTM D 638 | brk, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 1.2 GPa Show Supplier Material materials with Elastizitätsmodul of 1.2 GPa | ASTM D 638 | 50 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 587 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 587 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 33 MPa Show Supplier Material materials with Zugfestigkeit of 33 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 112 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 112 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C | ASTM D 648 | 3.2mm, unannealed |
Vicat-Erweichungstemperatur | 85 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 85 °C | ASTM D 1525 | Rate B/50 |
Wärmeformbeständigkeitstemperatur | 85 - 112 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 85 - 112 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Heavy Vehicles, Long Distance Coach, Recreational Vehicle | |
Availability | Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |