Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 48 MPa Show Supplier Material materials with Biegefestigkeit of 48 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 1.4 GPa Show Supplier Material materials with Biegemodul of 1.4 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | ISO 527 | yield, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 1.7 GPa Show Supplier Material materials with Elastizitätsmodul of 1.7 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 39 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 39 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 36 MPa Show Supplier Material materials with Zugfestigkeit of 36 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 113 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 113 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm |
Heat deflection temperature, 1.80 MPa | 84 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 84 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm |
Vicat-Erweichungstemperatur | 78 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 78 °C | ISO 306 | Rate B/50 |
Wärmeformbeständigkeitstemperatur | 84 - 113 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 84 - 113 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Heavy Vehicles, Long Distance Coach, Recreational Vehicle | |
Availability | Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |