Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.51 [-] Show Supplier Material materials with Relative Dichte of 1.51 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 225 MPa Show Supplier Material materials with Biegefestigkeit of 225 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 8.5 GPa Show Supplier Material materials with Biegemodul of 8.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 9.5 GPa Show Supplier Material materials with Elastizitätsmodul of 9.5 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 85 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 85 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 85 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 165 MPa Show Supplier Material materials with Zugfestigkeit of 165 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 900 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 900 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Relative temperature index, electrical | 180 °C Show Supplier Material materials with Relative temperature index, electrical of 180 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Entflammbarkeit | UL Recognized, 94-5VA Flame Class Rating: ≥1.2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.25mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221099- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=470961- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 1 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Technological properties
Property | ||
---|---|---|
Application areas | Data Transfer, Data Management, Circuit Protection, Air Cabin Interiors, EV Infrastructure, Forward Lighting, Enclosure/Housing/Cover, Enclosures, Electronic Components, Personal Computing, LED Lighting, Semiconductor, Wiring Devices, Wireless Communications | |
Availability | Europe,Asia,Americas | |
Processing methods | Hopper Temperature: 80 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |