Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 220 MPa Show Supplier Material materials with Biegefestigkeit of 220 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 9.2 GPa Show Supplier Material materials with Biegemodul of 9.2 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 9.2 GPa Show Supplier Material materials with Elastizitätsmodul of 9.2 GPa | ASTM D 638 | 5 mm/min |
Zugfestigkeit | 23.0 °C | 168 MPa Show Supplier Material materials with Zugfestigkeit of 168 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 900 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 900 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.62E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Relative temperature index, electrical | 180 °C Show Supplier Material materials with Relative temperature index, electrical of 180 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4.14E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 4.14E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Entflammbarkeit | UL Recognized, 94-5VA Flame Class Rating: ≥1.2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.25mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221099- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=470961- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Surgical Devices, Sensor, Pharmaceutical Packaging & Drug Delivery, Monitoring and Imaging, Medical Device, Personal Computing, Wireless Communications, Wiring Devices, Aircraft Exteriors, Building Accessory, Circuit Protection, Air Cabin Interiors, Aircraft Seating, Aerospace, Data Management, Data Transfer, Electronic Components, Enclosures, Electronics, Interior, Lab Ware and Clinical Diagnostics, Engine Component, Electronic Material Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Back Pressure: 0.3 to 0.7MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |