Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.41 g/cm³ Show Supplier Material materials with Dichte of 1.41 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 206 MPa Show Supplier Material materials with Biegefestigkeit of 206 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 7.1 GPa Show Supplier Material materials with Biegemodul of 7.1 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 2.9 % Show Supplier Material materials with Dehnung of 2.9 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 9.6 GPa Show Supplier Material materials with Elastizitätsmodul of 9.6 GPa | ASTM D 638 | 50 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 112 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 112 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 155 MPa Show Supplier Material materials with Zugfestigkeit of 155 MPa | ASTM D 638 | break |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Rear - Zone 1 Temperature: 265 to 275.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |