Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.47 g/cm³ Show Supplier Material materials with Dichte of 1.47 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 276 MPa Show Supplier Material materials with Biegefestigkeit of 276 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 12.1 GPa Show Supplier Material materials with Biegemodul of 12.1 GPa | ISO 178 |
Dehnung | 23.0 °C | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | ISO 527 | break, 5 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 13 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 74 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 74 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 189 MPa Show Supplier Material materials with Zugfestigkeit of 189 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 258 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 258 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.7E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Wärmeformbeständigkeitstemperatur | 258 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 258 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |